Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000590 GPa | 0.0856 ksi | |
BNZ Materials PA 20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |