Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00190 GPa | 0.275 ksi | dry |
Imerys Kingsleyâ„¢ Kaolin Kingsley is a coarse-grained, white firing kaolin used in the dinnerware, tile, artware and electrical porcelain industries.Information provided by Imerys |
|||
Modulus of Rupture | 0.00190 GPa | 0.276 ksi | EN 993-6: 1995 |
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Modulus of Rupture | 0.00190 GPa | 0.276 ksi | ASTM C133 |
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |