Polymer Property : Modulus of Rupture = 0.00241 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00241 GPa
0.350 ksi
Dry
Unifrax Fiberfrax® Pumpable-GS Pumpable Insulation
Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have te..
Modulus of Rupture 0.00241 GPa
0.350 ksi
Green (typ.)
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..