Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00259 GPa | 0.375 ksi | Dry |
Unifrax Fiberfrax® LDS AL-Moldable Moldable Insulation Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b.. |
|||
Modulus of Rupture | 0.00259 GPa | 0.376 ksi | Dipped Joint; ASTM C198 |
BNZ Materials Super Blakbond Mortar Super Blakbond is an air-setting mortar for general purpose plant use. It has greater air-setting strength than Blakbond or No. 2986. It is good for insulating fire brick where greater bond strength.. |