Mechanical Properties Metric English Comments
Modulus of Rupture 0.00400 GPa
0.580 ksi
EN 993-6: 1995
Skamol Group Moler M-EXTRA 'E' Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..