Polymer Property : Modulus of Rupture = 0.00447 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00447 GPa

@Temperature 375 °C
0.648 ksi

@Temperature 707 °F
Pyrotek Wollite 50 Insulating Castable
Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c..