Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00830 - 0.0103 GPa | 1.20 - 1.49 ksi | ASTM C133 |
Ceradyne Thermo-Sil® Castable 120 Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Modulus of Rupture | 0.00690 - 0.0103 GPa | 1.00 - 1.49 ksi | ASTM C133 |
Ceradyne Thermo-Sil® Castable TG Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |