Polymer Property : Modulus of Rupture = 0.0310 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0275 - 0.0310 GPa

@Temperature 815 °C
3.99 - 4.50 ksi

@Temperature 1500 °F
Pyrotek Pyrocast AL2 Abrasion-Resistant Refractory Castable
Pyrocast AL2 refractory castable is a mullite-based refractory well suited for applications prone to erosion and abrasion. It exhibits excellent non-wetting properties when used in molten aluminum ..