Mechanical Properties Metric English Comments
Modulus of Rupture 0.0689 GPa
9.99 ksi
Zircar Refractory Composites RS-200 Refractory Sheet
ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0689 GPa
9.99 ksi
Zircar Refractory Composites RS-201 Refractory Sheet
ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Modulus of Rupture 0.0689 GPa
9.99 ksi
Zircar Refractory Composites RS-202 Refractory Sheet
ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..