Polymer Property : Modulus of Rupture = 0.0870 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000600 GPa
0.0870 ksi
EN 993-6: 1995
Skamol Group V-1100 410 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Modulus of Rupture 0.000600 GPa
0.0870 ksi
Pyrotek Pyrocast PT-60 Castable Refractory
Pyrocast PT-60 is a ceramic fiber based insulating castable with very low thermal conductivity and excellent resistance to thermal shock.ApplicationsLaunder linings Distributor pan linings Ladle lin..