Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00103 GPa | 0.150 ksi | Green (typ.) |
Unifrax Fiberfrax® Duraboard® 2600 Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Modulus of Rupture | 0.00103 GPa | 0.150 ksi | Green (typ.) |
Unifrax Fiberfrax® Duraboard® 3000 Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |