Modulus of Rupture 0.00180 GPa
0.261 ksi
EN 993-6: 1995
Skamol Group Moler LR-1750 Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Modulus of Rupture 0.00180 GPa
0.261 ksi
EN 993-6: 1995
Skamol Group Moler SUPRA Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Modulus of Rupture 0.00180 GPa
0.261 ksi
EN 993-6: 1995
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..