Polymer Property : Modulus of Rupture = 0.265 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00183 GPa
0.265 ksi
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting
Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip..