Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0172 - 0.0200 GPa | 2.49 - 2.90 ksi | ASTM C133 |
Ceradyne Thermo-Sil® HS Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Modulus of Rupture | 0.0172 - 0.0207 GPa | 2.49 - 3.00 ksi | |
Pyrotek AFB-2300 HT Structural Board AFB-2300 HT is a ceramic fiber board which features a unique alumina-based binder. This white board is heat-treated to eliminate all possible out-gassing and withstands temperatures up to 1260°C.H.. |