Modulus of Rupture 0.552 GPa
80.0 ksi
Meehanite GC-40 Flake Graphite Cast Iron
Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d..