Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1U
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Eurotec® Tecomid® NB40 GR45 NL HS PA6, 45% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 110 kJ/m²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural
Information provided by Eurotec®