Polymer Property : Izod Impact, Unnotched (ISO) = 12.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 26.0 kJ/m²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
DuPont Performance Polymers Rynite® FR515 BK507 PET  (Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
Izod Impact, Unnotched (ISO) 26.0 kJ/m²

@Temperature -40.0 °C
12.4 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.