Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 14.6 kJ/m²

@Temperature 0.000 °C
6.95 ft-lb/in²

@Temperature 32.0 °F
Phr = 0
Shandong Rike Chemical HELIâ„¢ HL-35 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Izod Impact, Unnotched (ISO) 14.6 kJ/m²

@Temperature 0.000 °C
6.95 ft-lb/in²

@Temperature 32.0 °F
Phr = 0
Shandong Rike Chemical HELIâ„¢ HL-56 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Izod Impact, Unnotched (ISO) 14.6 kJ/m²

@Temperature 0.000 °C
6.95 ft-lb/in²

@Temperature 32.0 °F
Phr = 0
Shandong Rike Chemical HELIâ„¢ HL-57 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Izod Impact, Unnotched (ISO) 14.6 kJ/m²

@Temperature 0.000 °C
6.95 ft-lb/in²

@Temperature 32.0 °F
Phr = 0
Shandong Rike Chemical HELIâ„¢ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..