Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 16.0 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
7.61 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..