Polymer Property : Izod Impact, Unnotched (ISO) = 16.2 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 34.0 kJ/m²

@Temperature -40.0 °C
16.2 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1U
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched (ISO) 34.0 kJ/m²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled
SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 34.0 kJ/m²

@Temperature -30.0 °C
16.2 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled
SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 34.0 kJ/m²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled
SAXALEN PPH303G20 is a 20% glass filled Polypropylene - Homopolymer injection molding grade with good stiffness.Information provided by SAX Polymers