Polymer Property : Izod Impact, Unnotched (ISO) = 300 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 300 kJ/m²

@Temperature -30.0 °C
143 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 180/1U
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers