Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GR30 NL HW PA6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 95.0 kJ/m² @Temperature -30.0 °C |
45.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com.. |