Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 59.0 kJ/m²

@Temperature 23.0 °C
28.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber
Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Izod Impact, Unnotched (ISO) 59.0 kJ/m²

@Temperature 0.000 °C
28.1 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eU
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.