Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 181 kJ/m² @Temperature -30.0 °C |
86.1 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Izod Impact, Unnotched (ISO) | 181 kJ/m² @Temperature 23.0 °C |
86.1 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1U |