Polymer Property : Tensile Strength = 1160 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.00 MPa

@Strain 20.0 %,
Temperature 100 °C
1160 psi

@Strain 20.0 %,
Temperature 212 °F
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Tensile Strength 8.00 MPa

@Strain 20.0 %,
Temperature 100 °C
1160 psi

@Strain 20.0 %,
Temperature 212 °F
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..