Mechanical Properties Metric English Comments
Tensile Strength 117 MPa

@Temperature 23.0 °C
17000 psi

@Temperature 73.4 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
Tensile Strength 117 MPa

@Temperature 23.0 °C
17000 psi

@Temperature 73.4 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers
Tensile Strength 117 MPa

@Temperature 23.0 °C
17000 psi

@Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers