Polymer Property : Tensile Strength = 12.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 12.6 MPa

@Strain 300 %
1830 psi

@Strain 300 %
Type IV, 510 mm/min; ASTM D638
PolyOne Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..
Tensile Strength 12.6 MPa

@Strain 300 %
1830 psi

@Strain 300 %
Type IV, 510 mm/min; ASTM D638
PolyOne Elastamax™ HTE 3170 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..