Mechanical Properties Metric English Comments
Tensile Strength >= 827 MPa

@Thickness 0.254 - 0.635 mm
>= 120000 psi

@Thickness 0.0100 - 0.0250 in
ASTM E-8
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet
Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength >= 827 MPa

@Thickness 0.635 - 1.52 mm
>= 120000 psi

@Thickness 0.0250 - 0.0600 in
ASTM E-8
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet
Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength >= 827 MPa

@Thickness 1.52 - 2.29 mm
>= 120000 psi

@Thickness 0.0600 - 0.0900 in
ASTM E-8
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet
Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength >= 827 MPa

@Thickness 2.29 - 4.75 mm
>= 120000 psi

@Thickness 0.0900 - 0.187 in
ASTM E-8
H.C. Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet
Arc-Cast Sheet 3402Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength >= 827 MPa

@Thickness 4.762 - 12.7 mm
>= 120000 psi

@Thickness 0.1875 - 0.500 in
ASTM E-8
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate
Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..