Mechanical Properties Metric English Comments
Tensile Strength 190 MPa

@Thickness 0.102 mm
27600 psi

@Thickness 0.00400 in
RT; ASTM D638
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material
SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a ..
Tensile Strength 190 - 240 MPa

@Thickness 4.00 - 12.5 mm
27600 - 34800 psi

@Thickness 0.157 - 0.492 in
Temper H111; Standard EN 485-2
Constellium PLAN 5754 Aluminum Rolled Plate
Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m..
Tensile Strength 190 - 240 MPa

@Thickness 4.00 - 12.5 mm
27600 - 34800 psi

@Thickness 0.157 - 0.492 in
Temper H111; Standard EN 485-2
Constellium PLAN OX 5754 Aluminum Rolled Plate
Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone..
Tensile Strength 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers