Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 275 MPa @Temperature 600 °C |
39900 psi @Temperature 1110 °F |
|
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Tensile Strength | >= 275 MPa @Thickness 5.00 - 6.30 mm |
>= 39900 psi @Thickness 0.197 - 0.248 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength | >= 275 MPa @Thickness 100 - 150 mm |
>= 39900 psi @Thickness 3.94 - 5.91 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 275 MPa @Thickness 100 - 150 mm |
>= 39900 psi @Thickness 3.94 - 5.91 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | 275 MPa @Thickness 120 - 150 mm |
39900 psi @Thickness 4.72 - 5.91 in |
Typical Strength |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
Tensile Strength | >= 275 MPa @Thickness 100 - 140 mm |
>= 39900 psi @Thickness 3.94 - 5.51 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |