Polymer Property : Tensile Strength = 285 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 285 MPa

@Thickness 6.00 - 20.0 mm
41300 psi

@Thickness 0.236 - 0.787 in
Typical Strength
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug..
Tensile Strength 285 MPa

@Thickness 20.0 - 120 mm
41300 psi

@Thickness 0.787 - 4.72 in
Typical Strength
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug..