Mechanical Properties Metric English Comments
Tensile Strength 20.0 MPa

@Temperature 90.0 °C
2900 psi

@Temperature 194 °F
ASTM D638
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Tensile Strength 20.0 - 24.0 MPa

@Temperature 75.0 °C
2900 - 3480 psi

@Temperature 167 °F
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..
Tensile Strength 20.0 MPa

@Strain 5.00 %,
Temperature 100 °C
2900 psi

@Strain 5.00 %,
Temperature 212 °F
50mm/min
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Tensile Strength 20.0 MPa

@Strain 1.00 %,
Temperature 60.0 °C
2900 psi

@Strain 1.00 %,
Temperature 140 °F
ISO 527
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing