Polymer Property : Tensile Strength = 325 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 325 MPa

@Thickness 8.00 - 25.0 mm
47100 psi

@Thickness 0.315 - 0.984 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength 325 MPa

@Thickness 7.90 - 25.0 mm
47100 psi

@Thickness 0.311 - 0.984 in
Typical Strength
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..