Mechanical Properties Metric English Comments
Tensile Strength >= 338 MPa

@Temperature 200 °C
>= 49000 psi

@Temperature 392 °F
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH