Polymer Property : Tensile Strength = 345 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 345 MPa

@Temperature 1000 °C
50000 psi

@Temperature 1830 °F
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
Tensile Strength >= 345 MPa

@Temperature 21.1 °C
>= 50000 psi

@Temperature 70.0 °F
H.C. Starck Ultra 76 Alloy (Ta 2.5%W)
Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low..