Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 38.0 MPa @Temperature 121 °C |
5510 psi @Temperature 250 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 38.0 MPa @Temperature 149 °C |
5510 psi @Temperature 300 °F |
ASTM D 638 |
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat.. |
|||
Tensile Strength | 38.0 MPa @Strain 1.00 %, Temperature 100 °C |
5510 psi @Strain 1.00 %, Temperature 212 °F |
ISO 527 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |