Mechanical Properties Metric English Comments
Tensile Strength 390 MPa

@Diameter 55.0 - 100 mm
56600 psi

@Diameter 2.17 - 3.94 in
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Strength 390 MPa

@Diameter 55.0 - 100 mm
56600 psi

@Diameter 2.17 - 3.94 in
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Strength >= 390 MPa

@Thickness 7.90 - 12.5 mm
>= 56600 psi

@Thickness 0.311 - 0.492 in
Temper T451; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Tensile Strength >= 390 MPa

@Thickness 12.5 - 40.0 mm
>= 56600 psi

@Thickness 0.492 - 1.57 in
Temper T451; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Tensile Strength 390 MPa

@Thickness 203.2 - 254 mm
56600 psi

@Thickness 8.000 - 10.0 in
Typical Strength
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Tensile Strength >= 390 MPa

@Thickness 203.2 - 254 mm
>= 56600 psi

@Thickness 8.000 - 10.0 in
Tempers T651 / T652
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength >= 390 MPa

@Thickness 60.0 - 80.0 mm
>= 56600 psi

@Thickness 2.36 - 3.15 in
Temper T651
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..
Tensile Strength >= 390 MPa

@Thickness 80.0 - 120 mm
>= 56600 psi

@Thickness 3.15 - 4.72 in
Temper T651
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..