Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 290 MPa @Thickness 3.90 - 6.00 mm |
>= 42100 psi @Thickness 0.154 - 0.236 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 290 MPa @Thickness 6.00 - 12.5 mm |
>= 42100 psi @Thickness 0.236 - 0.492 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 290 MPa @Thickness 12.5 - 40.0 mm |
>= 42100 psi @Thickness 0.492 - 1.57 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 290 MPa @Thickness 40.0 - 80.0 mm |
>= 42100 psi @Thickness 1.57 - 3.15 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 290 MPa @Thickness 80.0 - 100 mm |
>= 42100 psi @Thickness 3.15 - 3.94 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 290 MPa @Thickness 7.90 - 12.5 mm |
>= 42100 psi @Thickness 0.311 - 0.492 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Tensile Strength | >= 290 MPa @Thickness 12.5 - 40.0 mm |
>= 42100 psi @Thickness 0.492 - 1.57 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Tensile Strength | >= 290 MPa @Thickness 40.0 - 80.0 mm |
>= 42100 psi @Thickness 1.57 - 3.15 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Tensile Strength | >= 290 MPa @Thickness 80.0 - 100 mm |
>= 42100 psi @Thickness 3.15 - 3.94 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |