Mechanical Properties Metric English Comments
Tensile Strength >= 310 MPa

@Thickness 4.00 - 6.00 mm
>= 45000 psi

@Thickness 0.157 - 0.236 in
Temper T651; Standard EN 485-2
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength >= 310 MPa

@Thickness 4.99 - 6.00 mm
>= 45000 psi

@Thickness 0.196 - 0.236 in
Temper T651; Standard EN 485-2
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..