Mechanical Properties Metric English Comments
Tensile Strength 46.0 MPa

@Temperature 204 °C
6670 psi

@Temperature 399 °F
ASTM D 638
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material
Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ..