Mechanical Properties Metric English Comments
Tensile Strength 393 MPa

@Temperature 200 °C
57000 psi

@Temperature 392 °F
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy
High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. ..
Tensile Strength >= 393 MPa

@Thickness 127 - 152.4 mm
>= 57000 psi

@Thickness 5.00 - 6.000 in
Tempers T851/T852)
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..