Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 68.0 MPa @Temperature 150 °C |
9860 psi @Temperature 302 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |