Mechanical Properties Metric English Comments
Tensile Strength >= 505 MPa

@Thickness 203.2 - 254 mm
>= 73200 psi

@Thickness 8.000 - 10.0 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength 505 MPa

@Thickness 180 - 200 mm
73200 psi

@Thickness 7.09 - 7.87 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..