Polymer Property : Tensile Strength = 75.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 75.0 MPa

@Strain 2.00 %,
Temperature 23.0 °C
10900 psi

@Strain 2.00 %,
Temperature 73.4 °F
50mm/min
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Tensile Strength 75.0 MPa

@Strain 5.00 %,
Temperature 60.0 °C
10900 psi

@Strain 5.00 %,
Temperature 140 °F
50mm/min
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Tensile Strength 75.0 MPa

@Strain 6.00 %,
Temperature 100 °C
10900 psi

@Strain 6.00 %,
Temperature 212 °F
5mm/min
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength 75.0 MPa

@Temperature 100 °C
10900 psi

@Temperature 212 °F
ISO 527
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..