Mechanical Properties Metric English Comments
Tensile Strength 58.6 MPa

@Temperature 175 °C
8500 psi

@Temperature 347 °F
ASTM D638
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide
Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ..