Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 86.5 MPa @Temperature 90.0 °C |
12500 psi @Temperature 194 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |