Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 65.5 MPa @Temperature 23.0 °C |
9500 psi @Temperature 73.4 °F |
ASTM D638 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Tensile Strength | 65.5 MPa @Temperature 23.0 °C |
9500 psi @Temperature 73.4 °F |
ASTM D638 |
Saint-Gobain Meldin® 7021 Isostatically Molded Graphite Filled Polyimide Melidin® 7021 is a self-lubricating thermosetting polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best for high t.. |