Polymer Property : Peel Strength = 15.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.40 - 2.63 kN/m

@Temperature 24.0 °C,
Time 173000 sec
8.00 - 15.0 pli

@Temperature 75.2 °F,
Time 48.0 hour
180°, Supported Vinyl/Wood
3M Fastbond™ 4213-NF Industrial Adhesive
3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when..