Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.41 kN/m @Temperature 24.0 °C, Time 259000 sec |
48.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Peel Strength | 8.41 kN/m @Temperature 24.0 °C, Time 259000 sec |
48.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Peel Strength | 8.41 kN/m @Temperature 60.0 °C |
48.0 pli @Temperature 140 °F |
Bell Peel, 1 hour @ 70°C/158°F, Conditioning: Dry; EN2243-2 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |