Polymer Property : Peel Strength = 55.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 9.64 kN/m

@Temperature 60.0 °C,
Time 605000 sec
55.0 pli

@Temperature 140 °F,
Time 168 hour
JRF, MIL-C-27725; AMS-S83318
3M AC-250 B-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read..
Peel Strength 9.64 kN/m

@Temperature 60.0 °C,
Time 605000 sec
55.0 pli

@Temperature 140 °F,
Time 168 hour
JRF/SW, Stainless Steel; AMS-S83318
3M AC-250 B-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read..